Shujun Gao
Shujun Gao
rice.edu üzerinde doğrulanmış e-posta adresine sahip
Başlık
Alıntı yapanlar
Alıntı yapanlar
Yıl
Scanning electrochemical microscopy study on the electrochemical behavior of CrN film formed on 304 stainless steel by magnetron sputtering
S Gao, C Dong, H Luo, K Xiao, X Pan, X Li
Electrochimica Acta 114, 233-241, 2013
502013
Characterization of electrochemical and passive behaviour of Alloy 59 in acid solution
H Luo, S Gao, C Dong, X Li
Electrochimica Acta 135, 412-419, 2014
472014
Formation of iron oxide and iron sulfide at high temperature and their effects on corrosion
S Gao, B Brown, D Young, M Singer
Corrosion Science 135, 167-176, 2018
382018
Electrochemical migration of Sn and Sn solder alloys: a review
X Zhong, L Chen, B Medgyes, Z Zhang, S Gao, L Jakab
RSC advances 7 (45), 28186-28206, 2017
342017
Passivity breakdown on copper: Influence of temperature
C Dong, F Mao, S Gao, S Sharifi-Asl, P Lu, DD Macdonald
Journal of the Electrochemical Society 163 (13), C707, 2016
272016
Synthesis of a duplex Ni-P-YSZ/Ni-P nanocomposite coating and investigation of its performance
H Luo, X Wang, S Gao, C Dong, X Li
Surface and Coatings Technology 311, 70-79, 2017
262017
Corrosion Behavior of Mild Steel in Sour Environments at Elevated Temperatures
S Gao, P Jin, B Brown, D Young, S Nesic, M Singer
Corrosion 73 (8), 915-926, 2017
212017
Corrosion behavior of the expandable tubular in formation water
S Gao, C Dong, A Fu, K Xiao, X Li
International Journal of Minerals, Metallurgy, and Materials 22 (2), 149-156, 2015
192015
Preparation and characterization of anticorrosion Ormosil sol–gel coatings for aluminum alloy
X Pan, J Wu, Y Ge, K Xiao, H Luo, S Gao, X Li
Journal of sol-gel science and technology 72 (1), 8-20, 2014
172014
Effect of High Temperature on the Aqueous H2S Corrosion of Mild Steel
S Gao, P Jin, B Brown, D Young, S Nesic, M Singer
Corrosion 73 (10), 1188-1191, 2017
132017
Electrochemical behavior and nonlinear Mott-Schottky characterization of a stainless steel passive film
S Gao, C Dong, H Luo, K Xiao, X Li
Analytical Letters 47 (7), 1162-1181, 2014
92014
Sensing application in the precursor region of localized corrosion by scanning electrochemical microscopy
H Luo, C Dong, S Gao, C Du, K Xiao, X Li
Rsc Advances 4 (100), 56582-56595, 2014
72014
A Unified Experimental Method and Model for Predicting Scale Inhibition
C Dai, Z Dai, F Zhang, Y Zhao, G Deng, K Harouaka, X Wang, YT Lu, ...
SPE International Conference on Oilfield Chemistry, 2019
52019
formation mechanisms of iron oxide and iron sulfide at high temperature in aqueous H2S corrosion environment
S Gao, B Brown, D Young, S Nesic, M Singer
Journal of The Electrochemical Society 165 (3), C171, 2018
52018
The influence mechanism of Fe3+ on corrosion behavior of Ti6Al4V in sulfuric acid solutions
L Wang, XQ Cheng, SJ Gao, XG Li, SW Zou
Materials and Corrosion 66 (3), 251-256, 2015
42015
Corrosion Electrochemical Behaviors of Titanium in HCl-acidizing Fluid Used in Natural Gas Exploitation
X Zhong, S Yu, J Hu, L Chen, Y Shi, Z Zhang, S Gao, D Zeng, T Shi
Int. J. Electrochem. Sci 12, 2875-2892, 2017
32017
Passive properties of magnetron-sputtered CrN film on AISI 304 stainless steel
S Gao, C Dong, X Cheng, K Xiao, L Wang, X Li
Corrosion 70 (6), 627-635, 2014
32014
PREPARATION AND CHARACTERIZATION OF ANTI-CORROSION SELF-HEALING AND HYDROPHOBIC COATING ON ALUMINUM ALLOY
P Xiaoming, W Junsheng, X Kui, G Shujun, P Lihong, T Ran, L Xiaogang
32013
铝合金表面缓蚀自修复疏水性膜层的制备与表征
潘晓铭, 吴俊升, 肖葵, 高书君, 裴礼鸿, 田然, 李晓刚
金属学报 49 (9), 1113-1120, 2013
32013
三种典型接地极材料在陕北土壤模拟溶液中的腐蚀行为
王森, 胡亚博, 李志忠, 高书君, 吉宏亮, 董超芳, 李晓刚
腐蚀与防护 34 (6), 485-488, 2013
32013
Sistem, işlemi şu anda gerçekleştiremiyor. Daha sonra yeniden deneyin.
Makaleler 1–20